Actual Certified Material Test Report
Alloy |
ER316LSI (AWS A5.9) |
Diameter |
.045" |
Heat Number |
8075 |
Date Entered |
9/17/2004 |
Entered By |
JLA |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
0.010 |
Boron (B) |
0.0014 |
Carbon (C) |
0.009 |
Chromium (Cr) |
18.620 |
Cobalt (Co) |
0.100 |
Copper (Cu) |
0.050 |
Manganese (Mn) |
1.710 |
Molybdenum (Mo) |
2.640 |
Nickel (Ni) |
12.190 |
Niobium (Nb) |
0.005 |
Nitrogen (N) |
0.044 |
Phosphorus (P) |
0.012 |
Silicon (Si) |
0.800 |
Sulfur (S) |
0.001 |
Titanium (Ti) |
0.005 |
Typical Certified Material Test Report
Alloy |
ER316LSI (AWS A5.9) |
Date Entered |
9/10/2012 |
Entered By |
BY |
CHEMICAL ANALYSIS: |
|
Boron (B) |
|
Carbon (C) |
0.03 |
Chromium (Cr) |
18.0-20.0 |
Copper (Cu) |
0.75 |
Manganese (Mn) |
1.0-2.5 |
Molybdenum (Mo) |
2.0-3.0 |
Nickel (Ni) |
11.0-14.0 |
Phosphorus (P) |
0.03 |
Silicon (Si) |
0.65-1.00 |
Sulfur (S) |
0.03 |
YIELD STRENGTH, ksi: 64 |
|
TENSILE STRENGTH, ksi: 90 |
|
% ELONGATION min: 37 |