Actual Certified Material Test Report
Alloy |
ER100S-1 (AWS A5.28) |
Diameter |
3/32" |
Heat Number |
4/945 |
Date Entered |
9/15/2004 |
Entered By |
JLA |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
.004 |
Carbon (C) |
.060 |
Chromium (Cr) |
.200 |
Copper (Cu) |
.160 |
Manganese (Mn) |
1.430 |
Molybdenum (Mo) |
.300 |
Nickel (Ni) |
1.630 |
Nitrogen (N) |
.006 |
Phosphorus (P) |
.008 |
Silicon (Si) |
.450 |
Sulfur (S) |
.006 |
Vanadium (V) |
.040 |
TiZr |
.010 |
Chemical Other |
O .006 |
Typical Certified Material Test Report
Alloy |
ER100S-1 (AWS A5.28) |
Date Entered |
9/12/2012 |
Entered By |
BY |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
0.10 |
Carbon (C) |
0.08 |
Chromium (Cr) |
0.30 |
Copper (Cu) |
0.25 |
Manganese (Mn) |
1.25-1.80 |
Molybdenum (Mo) |
0.25-0.55 |
Nickel (Ni) |
1.40-2.10 |
Phosphorus (P) |
0.010 |
Silicon (Si) |
0.20-0.55 |
Sulfur (S) |
0.010 |
Titanium (Ti) |
0.10 |
Vanadium (V) |
0.05 |
Zirconium (Zr) |
0.10 |
Chemical Other |
0.50 |
YIELD STRENGTH, ksi: 88 |
|
TENSILE STRENGTH, ksi: 100 |
|
% ELONGATION min: 16 |