Actual Certified Material Test Report
Alloy |
ER309LSI (AWS A5.9) |
Diameter |
.035" |
Heat Number |
21944 |
Date Entered |
9/3/2004 |
Entered By |
JLA |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
0.0060 |
Carbon (C) |
0.0160 |
Chromium (Cr) |
23.000 |
Copper (Cu) |
0.0500 |
Manganese (Mn) |
1.9500 |
Molybdenum (Mo) |
0.1000 |
Nickel (Ni) |
1`3.940 |
Niobium (Nb) |
0.0150 |
Nitrogen (N) |
0.0600 |
Phosphorus (P) |
0.0160 |
Silicon (Si) |
0.7400 |
Sulfur (S) |
0.0010 |
Titanium (Ti) |
0.0100 |
Vanadium (V) |
0.0900 |
Typical Certified Material Test Report
Alloy |
ER309LSI (AWS A5.9) |
Date Entered |
9/10/2012 |
Entered By |
BY |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.03 |
Chromium (Cr) |
23.0-25.0 |
Copper (Cu) |
0.75 |
Manganese (Mn) |
1.0-2.5 |
Molybdenum (Mo) |
0.75 |
Nickel (Ni) |
12.0-14.0 |
Phosphorus (P) |
0.03 |
Silicon (Si) |
0.65-1.00 |
Sulfur (S) |
0.03 |
YIELD STRENGTH, ksi: 64 |
|
TENSILE STRENGTH, ksi: 87 |
|
% ELONGATION min: 41 |