Actual Certified Material Test Report
Alloy |
ER309 / 309L (AWS A5.9) |
Diameter |
.045" |
Heat Number |
V16003 |
Trace Code |
71 |
Country of Origin |
INDIA |
Date Entered |
8/31/2022 |
Entered By |
MG |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.0220 |
Chromium (Cr) |
23.8500 |
Copper (Cu) |
0.3200 |
Manganese (Mn) |
1.8900 |
Molybdenum (Mo) |
0.2500 |
Nickel (Ni) |
12.4000 |
Nitrogen (N) |
0.1380 |
Phosphorus (P) |
0.0230 |
Silicon (Si) |
0.3600 |
Sulfur (S) |
0.0080 |
Ferrite WRC |
11 |
MATERIAL IS FREE FROM MERCURY CONTAMINATION |
|
MATERIAL CONFORMS TO ASME SECTION II, PART-"C" SFA5.9/SFA5.9M.EDITION 2019 |
|
MATERIAL CONFORMS TO AWS A5.9/A 5.9M : 2017, CLASSIFICATION ER-309L |
Typical Certified Material Test Report
Alloy |
ER309 / 309L (AWS A5.9) |
Date Entered |
8/7/2008 |
Entered By |
MJH |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.03 |
Chromium (Cr) |
23.0-25.0 |
Copper (Cu) |
0.75 |
Manganese (Mn) |
1.0-2.5 |
Molybdenum (Mo) |
0.75 |
Nickel (Ni) |
12.0-14.0 |
Phosphorus (P) |
0.03 |
Silicon (Si) |
0.30-0.65 |
Sulfur (S) |
0.03 |
YIELD STRENGTH, PSI AS WELDED 58,000 |
|
TENSILE STRENGTH, PSI AS WELDED 85,000 |
|