Actual Certified Material Test Report
Alloy |
ER4130 |
Diameter |
.045" |
Heat Number |
12/1609 |
Date Entered |
2/9/2005 |
Entered By |
dbf |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
.016 |
Carbon (C) |
.310 |
Chromium (Cr) |
.920 |
Copper (Cu) |
.140 |
Manganese (Mn) |
.540 |
Molybdenum (Mo) |
.210 |
Nickel (Ni) |
.030 |
Phosphorus (P) |
.0030 |
Silicon (Si) |
.240 |
Sulfur (S) |
.0060 |
Titanium (Ti) |
.004 |
Vanadium (V) |
.004 |
Typical Certified Material Test Report
Alloy |
ER4130 |
Date Entered |
7/28/2016 |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
.016 |
Carbon (C) |
.31 |
Chromium (Cr) |
.92 |
Copper (Cu) |
.21 |
Manganese (Mn) |
.52 |
Molybdenum (Mo) |
.20 |
Nickel (Ni) |
.05 |
Phosphorus (P) |
.005 |
Silicon (Si) |
.25 |
Sulfur (S) |
.005 |
Vanadium (V) |
.004 |
Tizr |
.004 |
CONDITION A: Tensile strength 145,000psi PWHY@1150F, Normalize 1550F and Temper @1050F Yield strength 130,000psi Elongation 11%-32RC |
|
CONDITION B: Tensile Strength 110,000psi PWHT @1150f Yield strength 90,000psi, Elongation 20%-26RC |
|
CONDITION C: Tensile Strength 178,000psi PWHT @1150F, Normalize 1650F and Temper 800F Yield strength 170,000psi, Elongation 7%-40RC |
Welding Material Sales certifies that the above chemical test results are correct and conform to the AWS specification stated as contained in the records of the company. The test report represents the actual attributes of the heat number furnished.
Brian W. DePaul