Actual Certified Material Test Report
Alloy |
ER80S-D2 (AWS A5.28) |
Diameter |
1/8" |
Heat Number |
4/1519 |
Date Entered |
8/25/2004 |
Entered By |
JLA |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
.002 |
Carbon (C) |
.075 |
Chromium (Cr) |
.03 |
Copper (Cu) |
.13 |
Manganese (Mn) |
1.84 |
Molybdenum (Mo) |
.46 |
Nickel (Ni) |
.04 |
Nitrogen (N) |
.006 |
Phosphorus (P) |
.009 |
Silicon (Si) |
.70 |
Sulfur (S) |
.009 |
Vanadium (V) |
.007 |
TiZr |
.100 |
Typical Certified Material Test Report
Alloy |
ER80S-D2 (AWS A5.28) |
Date Entered |
9/12/2012 |
Entered By |
BY |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.07-0.12 |
Copper (Cu) |
0.50 |
Manganese (Mn) |
1.60-2.10 |
Molybdenum (Mo) |
0.40-0.60 |
Nickel (Ni) |
0.15 |
Phosphorus (P) |
0.025 |
Silicon (Si) |
0.50-0.80 |
Sulfur (S) |
0.025 |
Chemical Other |
0.50 |
YIELD STRENGTH, ksi: 68 |
|
TENSILE STRENGTH, ksi: 80 |
|
% ELONGATION min: 17 |
Welding Material Sales certifies that the above chemical test results are correct and conform to the AWS specification stated as contained in the records of the company. The test report represents the actual attributes of the heat number furnished.
Brian W. DePaul