Actual Certified Material Test Report

Alloy

ER80S-D2 (AWS A5.28)

Diameter

3/32"

Heat Number

M30264

Date Entered

8/4/2004

Entered By

prl

CHEMICAL ANALYSIS:

Carbon (C)

0.0900

Copper (Cu)

0.2700

Manganese (Mn)

1.8500

Molybdenum (Mo)

0.4600

Nickel (Ni)

0.0100

Phosphorus (P)

0.0140

Silicon (Si)

0.5800

Sulfur (S)

0.0090

Typical Certified Material Test Report

Alloy

ER80S-D2 (AWS A5.28)

Date Entered

9/12/2012

Entered By

BY

CHEMICAL ANALYSIS:
(Single values are maximum)

Carbon (C)

0.07-0.12

Copper (Cu)

0.50

Manganese (Mn)

1.60-2.10

Molybdenum (Mo)

0.40-0.60

Nickel (Ni)

0.15

Phosphorus (P)

0.025

Silicon (Si)

0.50-0.80

Sulfur (S)

0.025

Chemical Other

0.50

YIELD STRENGTH, ksi: 68

TENSILE STRENGTH, ksi: 80

% ELONGATION min: 17

Welding Material Sales certifies that the above chemical test results are correct and conform to the AWS specification stated as contained in the records of the company. The test report represents the actual attributes of the heat number furnished.