Actual Certified Material Test Report
Alloy |
ER309 / 309L (AWS A5.9) |
Diameter |
.035" |
Heat Number |
V18007 |
Trace Code |
71 |
Country of Origin |
INDIA |
Date Entered |
3/25/2024 |
Entered By |
AV |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.0270 |
Chromium (Cr) |
23.4500 |
Copper (Cu) |
0.0400 |
Manganese (Mn) |
1.7000 |
Molybdenum (Mo) |
0.0300 |
Nickel (Ni) |
12.6000 |
Nitrogen (N) |
0.1450 |
Phosphorus (P) |
0.0240 |
Silicon (Si) |
0.3400 |
Sulfur (S) |
0.0100 |
Ferrite WRC |
7 |
EN 10204 TYPE 3.1 |
|
CONFORMS TO ASME SECTION II, PART "C" SFA5.9/SFA5.9M EDITION 2021 |
Typical Certified Material Test Report
Alloy |
ER309 / 309L (AWS A5.9) |
Date Entered |
8/7/2008 |
Entered By |
MJH |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.03 |
Chromium (Cr) |
23.0-25.0 |
Copper (Cu) |
0.75 |
Manganese (Mn) |
1.0-2.5 |
Molybdenum (Mo) |
0.75 |
Nickel (Ni) |
12.0-14.0 |
Phosphorus (P) |
0.03 |
Silicon (Si) |
0.30-0.65 |
Sulfur (S) |
0.03 |
YIELD STRENGTH, PSI AS WELDED 58,000 |
|
TENSILE STRENGTH, PSI AS WELDED 85,000 |
|
% ELONGATION IN 2" AS WELDED 36 |
Welding Material Sales certifies that the above chemical test results are correct and conform to the AWS specification stated as contained in the records of the company. The test report represents the actual attributes of the heat number furnished.
Brian W. DePaul