Actual Certified Material Test Report

Alloy

ER312 (AWS A5.9)

Diameter

1/8"

Heat Number

303001

Date Entered

9/2/2004

Entered By

JLA

CHEMICAL ANALYSIS:

Carbon (C)

0.1160

Chromium (Cr)

30.120

Copper (Cu)

0.1240

Manganese (Mn)

1.7900

Molybdenum (Mo)

0.1380

Nickel (Ni)

8.6100

Phosphorus (P)

0.0190

Silicon (Si)

0.4000

Sulfur (S)

0.0009

Typical Certified Material Test Report

Alloy

ER312 (AWS A5.9)

Date Entered

9/10/2012

Entered By

BY

CHEMICAL ANALYSIS:
(Single values are maximum)

Carbon (C)

0.15

Chromium (Cr)

28.0-32.0

Copper (Cu)

0.75

Manganese (Mn)

1.0-2.5

Molybdenum (Mo)

0.75

Nickel (Ni)

8.0-10.5

Phosphorus (P)

0.03

Silicon (Si)

0.30-0.65

Sulfur (S)

0.03

YIELD STRENGTH, ksi: 78

TENSILE STRENGTH, ksi: 109

% ELONGATION min: 45

Welding Material Sales certifies that the above chemical test results are correct and conform to the AWS specification stated as contained in the records of the company. The test report represents the actual attributes of the heat number furnished.

Brian W. DePaul