Actual Certified Material Test Report
Alloy |
ER70S-2 (AWS A5.18) |
Diameter |
1/8" |
Heat Number |
X93456 |
Date Entered |
4/27/2005 |
Entered By |
SJB |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
0.0680 |
Carbon (C) |
0.0600 |
Chromium (Cr) |
0.0300 |
Copper (Cu) |
0.2500 |
Manganese (Mn) |
1.1500 |
Molybdenum (Mo) |
0.0001 |
Nickel (Ni) |
0.0100 |
Phosphorus (P) |
0.0130 |
Silicon (Si) |
0.5200 |
Sulfur (S) |
0.0050 |
Titanium (Ti) |
0.0700 |
Vanadium (V) |
0.0001 |
Zirconium (Zr) |
0.0500 |
Typical Certified Material Test Report
Alloy |
ER70S-2 (AWS A5.18) |
Date Entered |
9/11/2012 |
Entered By |
BY |
CHEMICAL ANALYSIS: |
|
Aluminum (Al) |
0.05-0.15 |
Carbon (C) |
0.07 |
Chromium (Cr) |
0.15 |
Copper (Cu) |
0.50 |
Manganese (Mn) |
0.90-1.40 |
Molybdenum (Mo) |
0.15 |
Nickel (Ni) |
0.15 |
Phosphorus (P) |
0.025 |
Silicon (Si) |
0.40-0.70 |
Sulfur (S) |
0.035 |
Titanium (Ti) |
0.05-0.15 |
Vanadium (V) |
0.03 |
Zirconium (Zr) |
0.02-0.12 |
YIELD STRENGTH (ksi: 58) / TENSILE STRENGTH (ksi: 70) / ELONGATION (%min: 22) |
|
Typical Charpy V-Notch: 35 ft.-lb. At -20 deg F |
Welding Material Sales certifies that the above chemical test results are correct and conform to the AWS specification stated as contained in the records of the company. The test report represents the actual attributes of the heat number furnished.
Brian W. DePaul