Actual Certified Material Test Report
Alloy |
E316LT1-1/4 |
Diameter |
1/4" |
Heat Number |
S2961 |
Trace Code |
41 |
Country of Origin |
USA |
Date Entered |
10/21/2016 |
Entered By |
NH |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.0400 |
Chromium (Cr) |
18.5400 |
Copper (Cu) |
0.2000 |
Manganese (Mn) |
0.7100 |
Molybdenum (Mo) |
2.4100 |
Nickel (Ni) |
12.2800 |
Nitrogen (N) |
TYP 0.0500 |
Phosphorus (P) |
0.0210 |
Silicon (Si) |
0.7200 |
Sulfur (S) |
0.0090 |
Ferrite WRC |
92 |
CONFORMS TO ASME SEC II PART C 2010 ED. 2011AD. |
|
CERTIFICATE IN ACCORDANCE TO EN 10204 TYPE 3.1 |
Typical Certified Material Test Report
Alloy |
E316LT1-1/4 |
Date Entered |
9/11/2012 |
Entered By |
BY |
CHEMICAL ANALYSIS: |
|
Carbon (C) |
0.04 |
Chromium (Cr) |
17.0-20.0 |
Copper (Cu) |
0.75 |
Manganese (Mn) |
0.5-2.5 |
Molybdenum (Mo) |
2.0-3.0 |
Nickel (Ni) |
11.0-14.0 |
Phosphorus (P) |
0.04 |
Silicon (Si) |
1.0 |
Sulfur (S) |
0.03 |
TENSILE STRENGTH, ksi: 70 |
|
% ELONGATION min: 30 |