Actual Certified Material Test Report

Alloy

ER308 / 308L (AWS A5.9)

Diameter

.035"

Heat Number

S80520

Date Entered

3/29/2005

Entered By

KRK

CHEMICAL ANALYSIS:

Carbon (C)

0.0180

Chromium (Cr)

19.7800

Copper (Cu)

0.4200

Manganese (Mn)

2.0500

Molybdenum (Mo)

0.2100

Nickel (Ni)

9.7500

Nitrogen (N)

0.0280

Phosphorus (P)

0.0270

Silicon (Si)

0.3100

Sulfur (S)

0.0090

Ferrite WRC

12.600

Typical Certified Material Test Report

Alloy

ER308 / 308L (AWS A5.9)

Date Entered

8/7/2008

Entered By

MJH

CHEMICAL ANALYSIS:
(Single values are maximum)

Carbon (C)

0.03

Chromium (Cr)

19.5-22.0

Copper (Cu)

0.75

Manganese (Mn)

1.0-2.5

Molybdenum (Mo)

0.75

Nickel (Ni)

9.0-11.0

Phosphorus (P)

0.03

Silicon (Si)

0.30-0.65

Sulfur (S)

0.03

YIELD STRENGTH, ksi AS WELDED: 54

TENSILE STRENGTH, ksi AS WELDED: 75

% ELONGATION IN 2" AS WELDED: 35